Computer aided x-ray analysis for determining growth kinetics of γ'phase in nickel-based wrought superalloys

From

Risø National Laboratory for Sustainable Energy, Technical University of Denmark

Language: English
Publisher: De Gruyter
Year: 1993
Pages: 183-191
ISSN: 21910324 and 03346455
Types: Journal article
DOI: 10.1515/HTMP.1993.12.4.183