Journal article
Cold welding - fractographic investigation of the weld formation
Language: | English |
---|---|
Year: | 1997 |
Pages: | 361-366 |
ISSN: | 26890445 , 00967629 and 00432296 |
Types: | Journal article |
ORCIDs: | Bay, Niels |
DTU users get better search results including licensed content and discounts on order fees.