Internal water curing with Liapor aggregates

By Lura, Pietro1,2

From

Section for Building Materials and Geotechnics, Department of Civil Engineering, Technical University of Denmark1

Department of Civil Engineering, Technical University of Denmark2

Internal water curing is a very efficient way to counteract self-desiccation and autogenous shrinkage in high performance concrete, thereby reducing the likelihood of early-age cracking. This paper deals with early-age volume changes and moisture transport in lightweight aggregate concrete realized with wet lightweight aggregates.

Lightweight aggregate concrete mixtures with different degree of saturation and different particle size of the lightweight aggregates were studied and compared to normal weight concrete. Autogenous deformations, selfinduced stresses in fully restrained conditions, elastic modulus and compressive strength were measured.

Early-age expansion of the mixtures was greater the higher the degree of the saturation of the lightweight aggregates and the finer their particle size. The elastic properties and the earlyage expansion of the lightweight aggregate concrete were calculated with simple composite models, showing good agreement with the experimental findings.

Language: English
Year: 2005
Pages: 5-23
ISSN: 15744078 and 00467316
Types: Journal article

DTU users get better search results including licensed content and discounts on order fees.

Log in as DTU user

Access

Analysis